In situ imaging nanoindentation was used to characterize the mechanical properties of pure paint films on eight types of plywood-based flooring with different wear resistance...
Keywords: in situ imaging nanoindentation, mechanical properties, paint film, wear resistance, wood flooring
11/2006 | Holzforschung, Walter de Gruyter