Two possible mechanisms for the corrosion protection by conducting polymer coatings are discussed in this paper...
Keywords: Corrosion Protection, Conducting Polymers, Delamination, Kelvin Probe
11/2005 | Zeitschrift für Physikalische Chemie, Oldenbourg WissenschaftsverlagMedium-density fibreboard (MDF) is a wood-based composite made from lignocellulosic fibres bound together by synthetic resin...
Keywords: composite, Delamination, drilling, medium-density fibreboard (MDF)
05/2007 | Holzforschung, Walter de GruyterA study was performed on stone groundwood (SGW) pulps produced on a pilot scale. The behaviour of selected juvenile and mature Norway spruce wood samples was investigated...
Keywords: Delamination, fibre development, fibrillation, juvenile wood, mature wood, microfibril angle (MFA), S1 layer, S2 layer, scanning electron microscopy (SEM), stone groundwood (SGW), ultrastructure of the cell wall
08/2007 | Holzforschung, Walter de Gruyter